Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL PPX™ Resin PPX7115 - Americas - (PPE+PP) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL PPX™ Resin PPX7115 - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl PPX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
NORYL PPX™ 7115 resin is a non-reinforced alloy of polyphenylene ether (PPE) + polypropylene (PP). This injection moldable grade exhibits high modulus, high-temperature performance, excellent melt strength, impact resistance, hydrolytic and dimensional stability. NORYL PPX7115 resin is an excellent candidate for applications requiring high modulus and chemical resistance.

UL Yellow Card Link E121562-221243
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 12 cm³/10min ISO 1133
Température 260 °C -
Charge 5 kg -
ASTM Data
Indice de fluidité, MFI 14 g/10min ASTM D 1238
Température 260 °C -
Charge 5 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 1370 MPa ISO 527
Contrainte d'écoulement 35 MPa ISO 527
Déformation à la rupture 50 % ISO 527
ASTM Data
Module en traction 1240 MPa ASTM D 638
Module de traction d’élasticité 35 MPa ASTM D 638
Résistance de traction à la rupture 34 MPa ASTM D 638
Allongement d’élasticité 8 % ASTM D 638
Allongement à la rupture 125 % ASTM D 638
Module de flexion 1370 MPa ASTM D 790
Izod choc avec entaille, 1/8 in 534 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de ramolliss. Vicat, A 131 °C ISO 306
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 mm -
ASTM Data
DTUL à 66 psi 112 °C ASTM D 648
DTUL à 264 psi 85 °C ASTM D 648
Vicat température 86 °C ASTM D 1525
Propriétés diversesValeurUnitéNorme du test
Densité 990 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 60 - 65 °C -
Pré-séchage - temps 2 - 4 h -
L'humidité de traitement ≤0.02 % -
Température de la matière fondue 260 - 290 °C -
Température du moule 30 - 50 °C -
Zone 1 225 - 275 °C -
Zone 2 240 - 280 °C -
Zone 3 250 - 290 °C -
Vitesse de rotation de vis 20 - 100 rpm -
Contre-pression 0.3 - 0.7 MPa -
Caractéristiques
Transformation
Moulage par injection
Disponibilité régionale
Amérique du nord
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.